Hi all,

Is it possible to use the epoxy catch can (https://www.easycomposites.co.uk/cp1-resin-infusion-catch-pot-small) as a degassing chamber? 
By FLD - 6/11/2014 8:22:28 AM

I leave mine on full vacuum (pump running) for a couple of minutes.  I have found that its best to warm the two components separately prior to mixing and degassing.  If you do it cold then it foams up quite a bit.  Slightly warm and it just bubbles.