New to composites ,but been working on this tank on and off for a bit now.

The plug was made from polystyrene followed by a balsa skin and a thin skim of filler and acrylic paint.

Unconventionaly i just waxed the plug and layed up the bottom followed by the top and once cured the dremal came out to part the top and bottom pices from the plug.

ready to add the filler neck and fuel line nipple before some kevlar layers , the hole lot will be coated with creswell or flowliner before its joined back together and another layer of kevlar and finished off with a red / black carbon.
Attachments
026.jpg (221 views, 942.00 KB)
012.jpg (212 views, 1.00 MB)
014.jpg (201 views, 753.00 KB)
018.jpg (200 views, 1.00 MB)
Joe
Joe
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 310, Visits: 1.5K
Looks awesome Wink

 



 


    A $1000 electronic device will always protect a 10 cents fuse
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search