vacuum infusion with polyester resin


Author
Message
mhdghoul
mhdghoul
Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)Supreme Being (447 reputation)
Group: Forum Members
Posts: 49, Visits: 113
any one does vacuum infusion with polyester, i dont have epoxy at my contry and i do overlay with polyester and its working very good so i tried to go a step ahead and i bought everything from ec and i do the same steps , but i keep facing bubles ????

as for overlaying , you can watch my channel videos its perfect Smile

best regards

best regards mhd alghoul mhdghoul@hotmail.com youtube channel :atmospherejo link is http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Reply
jay,
jay,
Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)Forum Guru (74 reputation)
Group: Forum Members
Posts: 10, Visits: 28
you can get a slow cure thin polyester to vac but you need to tap the pressure at about - 8 psi due to the stiren content