mhdghoul
mhdghoul
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 113
any one does vacuum infusion with polyester, i dont have epoxy at my contry and i do overlay with polyester and its working very good so i tried to go a step ahead and i bought everything from ec and i do the same steps , but i keep facing bubles ????
as for overlaying , you can watch my channel videos its perfect
best regards
best regards mhd alghoul 
mhdghoul@hotmail.com
youtube channel :atmospherejo link is
http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Reply
Like
3
Replies
mhdghoul
mhdghoul
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 49,
Visits: 113
best regards mhd alghoul 
mhdghoul@hotmail.com
youtube channel :atmospherejo link is
http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Reply
Like
3
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
Till now I did al my infusions with polyester
... its a very fluid polyest specialy made for surfboards i use
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
vacuum infusion with polyester resin
mhdghoul
-
13 Years Ago
:(
mhdghoul
-
13 Years Ago
Till now I did al my infusions with polyester :)... its a very fluid polyest specialy made for...
matthieutje65
-
13 Years Ago
you can get a slow cure thin polyester to vac but you need to tap the pressure at about - 8 psi due...
jay,
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search