I'm pretty new to using GC50 and have a question regarding the repair of a cosmetic part made with GC50.

When I've repaired gel coats before in the past, I've just mixed in wax and brushed it on, however I've heard that gc50 doesn't like being brushed and that it doesn't stick to itself very well.

Has anyone got any info on this? Luckily it's just one side of the part so if I have to I'll just brush epoxy over it an hope it doesn't yellow too quick, although it's off to Dubai so want to do it properly
Replies
SebRS
SebRS
Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)Supreme Being (245 reputation)
Group: Forum Members
Posts: 29, Visits: 558
Did you mixed it with any kind of additive? Or exactly same as you mixe it for making a new part?

Thanks.
Edited 11 Years Ago by SebRS
Brian_s
Brian_s
Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)Supreme Being (793 reputation)
Group: Forum Members
Posts: 99, Visits: 2.5K
I only mixed a small amount. Maybe 5 grammes so guessed that about 2 drips of MEKP would do.

Brian.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search