Hi guys
For those of you how are experienced this is probably a stupid question but I'm gonna ask anyway as I suspect it is something many struggle with.
What is your technique for getting a good finish on your plug?
I have a GF part which I want to take mould from, this is it although I have worked at it since these photos were taken.




I wanted to make a copy of my cracked instrument binnacle but it was very textured so I smoothed it as best I could and made a mould from it (actually I made four as this was my
first ever go at doing this and I didn't really know what I was doing) I then made a GF part from the least worst of the moulds and set about smoothing it. I started with 120 grit, then went on to 400, 800 and 1200.
My plan is to take this part which apart from the scratches I am happy with and make a new mould in two or three parts (advise on this very welcome) so that I can make CF copies which I hope to sell.
I thought it was going well until I rubbed it with cutting compound to a nice shiny finish but when I looked closely it was covered in lots of scratches, probably from the last two grits.

So, do you wet sand or dry sand?
How can you tell when you have sanded away the marks left by the previous grit? I dried it and thought they were gone but apparently not.
Do you use a DA sander, a block or just hold the paper?
How long do you normally spend smoothing a part like this, I spent a whole evening at it and will probably need to spend another one to get rid of the fine scratches.
How smooth a finish is realistic on Gel coat?

Thanks in advance
Ali
Edited 11 Years Ago by Alibro
Reply
tack talk
tack talk
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 215
p120 is a harsh grade to start with.  It will leave some very deep scratches which will likely be difficult to completely remove later with the finer grades.

I would start with a less severe grade than P120 then work through the grades making sure that the gap between the grades is never to large e.g. P400 to P600 to P800 to P1200. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago
Hanaldo - 11 Years Ago
Alibro - 11 Years Ago
The Fibreglass King - 11 Years Ago
Hanaldo - 11 Years Ago
Warren (Staff) - 11 Years Ago
Alibro - 11 Years Ago
FLD - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
tack talk - 11 Years Ago
Alibro - 11 Years Ago
Hanaldo - 11 Years Ago
Warren (Staff) - 11 Years Ago
Alibro - 11 Years Ago
Hanaldo - 11 Years Ago
FLD - 11 Years Ago
brainfart - 11 Years Ago
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago
ajb100 - 11 Years Ago
Alibro - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search