question gloss finish release agent


Author
Message
bip
bip
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 8, Visits: 12
Hello

I would like to the parts to have a high gloss finish, can easy lease chemical release agent do that ? 
Question is how high gloss is that ?  like a piano gloss ? or something like the attached ? 
How hard is the finish ? scratch prove? can the scratch be easliey buff off by polishing it ? 
Thanks 
  http://www.talkcomposites.com/Uploads/Images/c2a8108c-45a6-4cab-b42a-04ab.jpg
Reply
bip
bip
Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)Supreme Being (98 reputation)
Group: Forum Members
Posts: 8, Visits: 12
I'm using alumimun mould now, so surface wise should be fine, 
but what about "sand holes" ? or air bubbles ?  
Is this agent thick enough to cover them up ? 
Also parting line on the mould , the perssure of the autoclave will push what ever there is to those line
Thanks 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search