Rob
Rob
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 7
Hi,
I'm a sculptor making wood sculpture and want to protect it from the elements. Does anyone have any recommendations about which resin I should use?
Thanks
Rob
Reply
Like
2
fgayford
fgayford
posted 11 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
Hi Don't even think about coating it with resin, it will peel off. Boat guys have a tried and true way to protect wood from the sun. Spar Varnish.
Fred
Reply
Like
1
brainfart
brainfart
posted 11 Years Ago
ANSWER
Post Details
Group: Forum Members
Posts: 198,
Visits: 1.4K
I strongly disagree! Epoxy resins are very good at protecting wood from water, and the boatbuilding community has very good paints and clear coats to protect the epoxy from UV.
http://www.toolbase.org/Best-Practices/Failure-Prevention/protecting-wood-from-humidity
"Molten paraffin wax and a sheathing grade, two-component epoxy
material with no solvent were the very best finishes found in
this study for controlling moisture vapor movement into
wood. The MEE is a direct function of the number of coats
of finish applied to the wood (film thickness) and the length
of time of exposure to a particular humidity"
www.fpl.fs.fed.us/documnts/fplrp/fplrp462.pdf
Three coats of epoxy will keep the water out.
Reply
Like
1
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search