Hi all,

Still playing around trying to make my wheel spats. My moulds are made from ec epoxy  tooling gel coat and I've been using easylease release agent. One of my moulds has had 3 parts out of it now but what im noticing each time I de mould is that the glossy surface of the mould is left with a pattern of the cloth which I assume is traces of cured resin. Each time I've washed the moulds in soap and water and also used mould cleaner  try and remove it and then re applied the easylease as from scratch. Is this normal with wet lay up/vacuum bagging or am I going wrong??

How critical is the shelf life of easylease?, Mine (foolishly) came of ebay, the tin hadn't been opened but its age is anyones guess!!.  

Cheers

Craig
Replies
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I get the same pattern on my moulds, it's nothing to be concerned about. You don't need to wash it off, I just buff mine lightly with a clean cloth after each pull and then do one wipe with my release agent which is Frekote. This pretty much eliminates the pattern on the mould surface, and what does remain doesn't transfer to any parts. 
craig81
craig81
Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)Forum Guru (65 reputation)
Group: Forum Members
Posts: 11, Visits: 933
Great, thanks for all the help everyone, the bits left behind in mine do feel more than just a film, the tiny bits pick off with your nail. I'll have another go, concentrating on by bag seal and perhaps leave it longer before de moulding.

Cheers
Craig
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
craig81 - 11 Years Ago
matthieutje65 - 11 Years Ago
craig81 - 11 Years Ago
matthieutje65 - 11 Years Ago
ajb100 - 11 Years Ago
carbonfibreworks - 11 Years Ago
craig81 - 11 Years Ago
carbonfibreworks - 11 Years Ago
ajb100 - 11 Years Ago
Hanaldo - 11 Years Ago
craig81 - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search