Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
I get the same pattern on my moulds, it's nothing to be concerned about. You don't need to wash it off, I just buff mine lightly with a clean cloth after each pull and then do one wipe with my release agent which is Frekote. This pretty much eliminates the pattern on the mould surface, and what does remain doesn't transfer to any parts.
|