Hi all, I'm looking to make some side skirt splitters (basically long planks of carbon). So could I make a mould out of mdf and use resin infusion? I would make a positive mould (if that's the correct word), and make the mdf the shape of the inside of the finished part and lay carbon over the top of it. I'm trying to make it as cost effective as possible, while keeping the quality high

Reply
dbcrx
dbcrx
Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)Supreme Being (362 reputation)
Group: Forum Members
Posts: 46, Visits: 1.2K
If you want to make the mold the inside of the piece (the side that won't be seen) then all you have to do is cover it in packing tape and lay your fabric. It will release easily, but you'll have to finish the visible side by flow coating and clearcoating.