Hi all, I'm looking to make some side skirt splitters (basically long planks of carbon). So could I make a mould out of mdf and use resin infusion? I would make a positive mould (if that's the correct word), and make the mdf the shape of the inside of the finished part and lay carbon over the top of it. I'm trying to make it as cost effective as possible, while keeping the quality high