Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Connecting tubing
Connecting tubing
Post Reply
Like
3
Connecting tubing
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
mattv
mattv
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 3,
Visits: 26
Hi ,
I'm just about to connect 2 half metre lengths of 32mm ID CF Tube using a 300mm length of 28.5mm ID CF Tube inside .
I'm going to use PT326 , but what i want to know is how much of the Structural epoxy to use to make it solid into one piece,
also what type of preparation do i need to do on the tubes .Is it just on the inside of the 32 mm or do i need to sand the outer surface
of the 28.5 tube .
Also any tips on how to get at least 15cm down into the tube to sand ?
Bit of a newbie at all this .
cheers M
Reply
Like
3
Reply
Hanaldo
Hanaldo
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Acetone. I'd give it a wash with soap and water first, then wipe it all down with acetone. Then scuff the surfaces up really well, followed by another heavy wipe with acetone.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Connecting tubing
mattv
-
11 Years Ago
Prep all surfaces to be bonded, so inside of the 32mm and outside of the 28.5mm. Easy enough to...
Hanaldo
-
11 Years Ago
Make double sure your preparation and keying of the surfaces is spot on. Roll wrapped tubes are made...
Warren (Staff)
-
11 Years Ago
That's great, thanks guys , a little bit of experimenting with the glue amounts I guess . What's the...
mattv
-
11 Years Ago
Acetone. I'd give it a wash with soap and water first, then wipe it all down with acetone. Then...
Hanaldo
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search