Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Advice on best resin for front panel detailing
Advice on best resin for front panel detailing
Post Reply
Like
3
Advice on best resin for front panel detailing
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Noblea
Noblea
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 3
Hi,
I looking for some advice on what would be the best type of resin for a project I'm planning.
The project requires a front panel which I plan to cut from either a solid wood or ply-board using a laser cutter. Then using a technique that I saw during the manufacture of police badges, I'd like to fill the lettering indentations, cut from the laser, with a white coloured resin using a syringe. Once cured I will sand the panel flat and give the wood a dark coloured stain. This will hopeful give me a professional looking front panel with the white lettering set out against the dark grain of the wood.
As a resin novice my question is which type of resin and pigment would be best for this application?
Thanks,
Noblea
Reply
Like
3
Reply
Warren (Staff)
Warren (Staff)
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
The easiest way would be to use our
Fast-Cast Polyurethane Casting Resin
and one of our
Polyurethane Colour Pigment
You can mix in the white pigment to get the colour you want. The advantage is it is quick curing and is fine when sanded with wood.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Advice on best resin for front panel detailing
Noblea
-
11 Years Ago
The easiest way would be to use our Fast-Cast Polyurethane Casting Resin and one of...
Warren (Staff)
-
11 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search