Hanaldo
Hanaldo
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Hey guys,
I recently ordered some Biotex Flax and Jute fabrics from you for a little experiment that I am doing, but I just wanted to inquire about the fabrics stiffness. I have read that the fabrics are similar to fibreglass in terms of stiffness, is that so?
If I wanted to make a flat sheet approx. 500x300mm, to carry a small weight load (say 5kg, to be safe) without any flex, how many layers of the fabric would I need to use?
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Biotex Flax
Hanaldo
-
12 Years Ago
as far as I did tests with flaxfiber you'll need "some" layers... its indeed similar to fiberglass...
matthieutje65
-
12 Years Ago
Hmm, bit more than I was hoping for. I might use some strips of carbon in the middle of the layup...
Hanaldo
-
12 Years Ago
As you say Soric negatively effects the natural colour of the flax. I have tried adding dye to the...
wozza
-
12 Years Ago
Thanks Warren. Do you think if I used a layer, or rather strategically placed strips of carbon fibre...
Hanaldo
-
12 Years Ago
Adding carbon to the centre of a laminate won't do much for stiffness as it is the neutral layer at...
Fasta
-
12 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search