	Group: Administrators 	        
    Posts: 2.5K, 
    Visits: 8.5K 
    
 
          
		     | 
				                       
                 
                
                    
			            HI,
  The 20mm box section does not have any CAD drawings available to us.  It is not massively precise.  The internal radii seems to vary between 3.6 and 3.8mm.  The outer radii varies between 4.8 and 5.2mm.  That has been measured by hand.                
			            
  				