Hi this is not my first part but i keep messing up when mixing up the resin could sumone please help me with how much resin i would need for a flat part measuring 3ft x 2ft made of 200g carbon, 3 layers of 290g woven glass,peel ply and mesh?
Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Jdmleesy (08/04/2014)
Even with the easy composites resin ?


Yep.

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Jdmleesy - 11 Years Ago
ChrisR - 11 Years Ago
ajb100 - 11 Years Ago
Jdmleesy - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
Jdmleesy - 11 Years Ago
ajb100 - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Jdmleesy - 11 Years Ago
wozza - 11 Years Ago
Jdmleesy - 11 Years Ago
wozza - 11 Years Ago
Hanaldo - 11 Years Ago
wozza - 11 Years Ago
Jdmleesy - 11 Years Ago
wozza - 11 Years Ago
Jdmleesy - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search