Nope, standard practice. Just make sure everything is well degreased and stuck down. Lay a few mist coats down first before building up to heavier coats. Lay the clear down too heavy too quickly and the clear can creep under the edges and lift the vinyl. Hope that helps.
Warren
Carbon Copies Ltd
|