i saw a picture of a section of carbon fibre "tunnel" that had an interior carbon fibre hexagon core. at first i thought ok so he made some hexagon box lengths, glued them together, then wrapped it up in another layer. then i noticed a curve in the tunnel. ive drawn a terrible pic to demonstrate what it was like.

how the f**k was this done? 
Attachments
ddd.png (256 views, 4.00 KB)
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Not totally sure I understand what you're describing, but I'm gonna guess it was simply done with this specialty Honeycomb weave pattern? 

coleio
coleio
Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)Supreme Being (418 reputation)
Group: Forum Members
Posts: 68, Visits: 285
no, ok think of the entire structure as a beam, with a radius of say 20cm, and a length of 1m with a curve at the end like in the drawing. the outer wall is 2mm thick. within the outer walls are honeycomb tunnels, running from one end to the other with a wall thickness of .8mm. get me?