By cbk - 4/4/2019 2:11:13 PM
What is the fibre volume fraction of XC110 prepreg?
|
By Warren (Staff) - 10/11/2019 9:18:19 AM
Follow the Low Temp Cycle in the XC110 processing guide as that has a maximum cure temperature of 85C which is within your limits. However it is not a single stage process.
|
|