Talk Composites - The Forum for Advanced Composites

Whats the point of sanding after first coat?

http://www.talkcomposites.com/Topic23662.aspx

By Interloper393 - 7/15/2017 2:45:47 PM

Hi guys,  after your very first coat in the video you sand the part,  if it's a flat piece or there's no joins ect is there any need to sand or can you just add more coats after it gets to the tacky stage.

Cheers
By Hanaldo - 7/18/2017 12:42:32 AM

I thought so, but theres a couple of videos that they sand something so thought best to clarify! 

The main reason for sanding is to de-nib, so you get rid of any sharp edges, dry fibres, etc. If what you are doing is flat or a simple shape, then there's no reason you can't skip the sanding provided you're still within that 'tack-free' window.