By mentallykilled - 5/29/2012 2:40:49 PM

so this isnt your typical car carbon fibre questions.

im after making a les paul guitar copy in carbon fibre.
http://images.gibson.com/Files/20b17b4b-a49a-4567-bd13-f55bbbaf7850.jpg (for anyone that doesnt know)

im just after some general advice on what could be the best way for me to do it, i was thinking of skinning the guitar so i could make the back & sides of the guitar and neck in 1 piece, then skin the top and somehow bond the top to the bottom (this is a big bit im unsure of how best to do)

the other options making a mould on the cnc machine of the guitar and doing it that way which would be very precise and would leave me an area to have an overrun of fabric so can trim back to an accurate shape but still leaves the problem of bonding the top to the bottom so we have a light-weight guitar

also what would you recommend for the strength of it, i was thinking of using a heavy gsm carbon fibre for a reinforment layer then laying a 220gsm over top for a nice decorative layer.

am i going to need diamond coated blades for cuttings i do with this? (probably silly question)

thanks in advance
By Warren - 5/31/2012 6:13:31 PM

The "lost foam" method is good for one offs or if you want no joins. You in effect carve yourself a plug out of styrofoam (it must be styrofoam).  Then using epoxy based resins you lay over your layers of carbon and wet it out in the same technique you would do for simple wet lay techniques. You then lay up ideally some coating resin like found in the bonnet skinning kits to build up resin to give you a surface you can sand smooth. once the thing is properly cured, you pour acetone into the middle through a hole and the acetone will dissolve the foam. You can then just pour out the liquid leaving a hollow carbon shape.

You cant use polyester resin as it will dissolve the resin.  Also you must ensure the epoxy is cured before you play with acetone as uncured epoxy can be broken down with acetone.


You wont get far using kitchen scissors to cut carbon! they will snag easy and blunt real quick.  decent carbon shears cut through carbon real easy.