By kylec - 2/17/2015 12:36:51 PM
Hi,
I found some Nomex/Kevlar honeycomb sheets in our warehouse and it has been there for a few years. Is this honeycomb still usable and how can I tell? It has been stored indoors the whole time with a plastic cover over it (it is not sealed). How does honeycomb degrade over time? How should it be stored to prevent further degradation?
Any help is most appreciated!!!!
Thank you!
|
By Julien - 2/17/2015 2:08:14 PM
Hi,
I don't exactly know the shelf life, but if you want to use it, begin by heat your honeycomb core in a oven to remove the water/humidity accumulated during years.
Nomex is a material that easily absorb humidity...
|
|