Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
pva and wax
pva and wax
Post Reply
Like
3
pva and wax
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
mhdghoul
mhdghoul
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 113
guys all i got here is a clear color pva and i want blue or whatever color i could get to trace it on the mold , can anyone help me and tell me what kind of color can i add without harming the pva?
as for the wax , which is the best wax i can find in a local store that can be used for waxing molds.
best regards mhd alghoul 
mhdghoul@hotmail.com
youtube channel :atmospherejo link is
http://www.youtube.com/user/atmospherejo?ob=0&feature=results_main
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
pva and wax
mhdghoul
-
13 Years Ago
Hi, For waxing your plug or mold, pure carnauba wax will work. You can find it at any car shop....
Joe
-
13 Years Ago
answering any question is helpful , really thank u ill try it as for the wax , the problem is me not...
mhdghoul
-
13 Years Ago
Use any water based ink to add colour to PVA.
workaholic_ro
-
13 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search