The problem with such big "ice" systems is not just sound deadening but flexing of the panels itself, hence the need to stiffen the panel up.
The aluminium box section example does look a bit ropey.... That said, if he bonds in the honeycomb and skins it properly then there is no reason why it shouldnt be structurally sound.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|