hi all,

just on a rough guide how much resin would be required if i was using approx

Carbon Fibre Plain Weave 3k 200g 1m Wide x 3m length

how much would i need

Epoxy Coating Resin 1kg Pack and Carbon Skinning Basecoat 1kg Pack

to be more than enough to cover the whole bumper in base coat and x 2/3 layers of coating resin?

 

im thinking of skinning my complete front bumper for a vectra b GSI

many thanks

phil

 
Edited 14 Years Ago by Warren
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search