Before placing an order (asap, march 07) I would like air these thoughts.
It all concerns making a mold for the tank/seat part in the picture,
the final part will be made with epoxy and carbon.
In the past I have always made polyester based molds, and yes I have mostly
produced polyester parts in them, but a few times epoxy based parts with
good result and no problem with release. (letting the molds air for a while)

But the question is, would you strongly recommend to make epoxy molds for epoxy parts?
And if so, is the components in the "Epoxy Mould Making Kit" suitable for something in this size?
(We plan to buy the gelcoat and putty separately, not the kit)
Would it be a good idea to ad extra reinforcement, chopped strand mat,
to get extra strength?
Would adding that with EL2 on top of the putty work?
Would skipping the putty and only use gelcoat and EL2 work? (with chopped strand mat).


http://www.motoform.se/images/portf/nc30motoform.jpg

Also, when making the actual part that we plan to envelope bag,
is the EL2 slow, the slowest epoxy you have?
We feel that time will run out whilst laying up carbon and peel etc
on this "large" part.
I can work in a slightly lower temperature, that should slow things down right?

Hoping for a quick reply.
Thank you.


http://motoform.blogspot.se

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search