Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
How many layers for 3cm flat sheet?
How many layers for 3cm flat sheet?
Post Reply
Like
9
How many layers for 3cm flat sheet?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 380
I want to make a flat sheet (or rather block) of carbon fiber that is 3cm thick? It's not a big block, roughly 7x7cm. I can only imagine infusion would be pretty useless for this as vacuum will have hard time pushing down that thick of a sheet so I'm thinking wet lay up and put something really really have on top to compress. What say you? Also, most importantly, how many layers do you think i'm gonna need to build that kind of thickness?
Regards,
Stan
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How many layers for 3cm flat sheet?
StanTheMan
-
12 Years Ago
Anybody? I'm most likely to be using 285gsm 4x4 twill if that''s of any significance
StanTheMan
-
12 Years Ago
Hi, Normally I get around 1 mm thickness from 4 layers of 200 gsm twill .. I would simply do a...
Dravis
-
12 Years Ago
Because I want to make a watch case from the block. The watch case itself will be 44mm but I need...
StanTheMan
-
12 Years Ago
I disagree with the weight point. aluminium is about 2.7gm/cm3 where as carbon is 1.6-1.8 gm/cm3...
Warren (Staff)
-
12 Years Ago
As a very general rule with vac bagging, I read 200gsm is between .25 and .3mm thick
ajb100
-
12 Years Ago
With regards to the weight point, I think you're right Warren, but I was thinking more in terms of...
Dravis
-
12 Years Ago
[quote][b]Dravis (31/01/2014)[/b][hr]With regards to the weight point, I think you're right Warren,...
StanTheMan
-
12 Years Ago
I like the forged carbon idea, easy to make a part in the end but the tooling and set up could be...
Fasta
-
12 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search