It happens all the time, if you get the chance trya nd get to a boat builders when they are removing the hull from the mould... propper thunder and lightning indoors!
20_rc51_00
20_rc51_00
Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)Supreme Being (683 reputation)
Group: Forum Members
Posts: 95, Visits: 548
I have noticed this on my breathe-right nasal strips when i remove the adhesive backing and also with some resins too. I would guess it's most likely due to the resin being delaminated, most likely the result of energy release and electrons jumping to lower energy levels likely to do with the breakage of chemical bonds (based on my rusty chemistry background some long time back, this is common for organic/polymeric compounds)
StanTheMan
StanTheMan
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 61, Visits: 380
Thing it never happened before. And it's a resin I've used before. At first I thought I was seeing things because the room was a little dim. But then on the second pull I was like WOAH!!!
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
seen it once before and nobody believed me BigGrin probably static electricity caused by friction between the peelply and carbonfiber Smile like you have with a sweater sometimes

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




StanTheMan
StanTheMan
Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)Supreme Being (455 reputation)
Group: Forum Members
Posts: 61, Visits: 380
I was removing the peel ply and infusion mesh on a part today only to notice this happening. WTH?!?!