I've recently been doing a repair which has required the use of epoxy resin and ET515 to stick the bits back together. Unfortunately I was unable to post cure a lot of the carbon parts prior to applying 515 to places.

Now I'd like to post cure the whole thing but I'm just wondering what effect the post cure will have on the 515. I'm only planning to go to around 60-70'c but looking at the graph in the technical data sheet, this is past it's stable operating temperature.

There won't be any load on it during post cure but will it return to full strength once it has cooled or will taking it past 40'c do irreversible damage?

Thanks in advance
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search