ANSWER
Topic Details
Group: Forum Members
Posts: 20,
Visits: 102
Hi,
I have made a mould for some headlight covers which I intend to layup using resin infusion, however there are some blemishes in the surface and the 'barriers' due to chips in the parts I have taken the mould from, along with a crack due to a slight gap between my plasticine barrier and the original part.
Is it best to fill these using the Unimould Tooling Gelcoat (will it set if left out in the open?) or should/could I use the High Gloss Pattern Coat?
Thanks
MacG Racing Ltd.
, UK based Motorsport Racing Team - follow us on
Twitter
and on
Facebook
Reply
Like
1
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Voids in Unimould surface
macgtech
-
11 Years Ago
Yes use the tooling gel coat and then you have two options to ensure it cures and one is to use this...
carbonfibreworks
-
11 Years Ago
That's great, thanks very much
macgtech
-
11 Years Ago
Post Reply
Like
1
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search