Hi Everyone:

I am a newbee so I suspect this will take many tries. I wish to make a kayak paddle out of carbon fiber that has a foam core - so heres my confusion

I have existing paddle and will make a split fiberglass mold.

OK so I have the mold - I can layup carbon on each side  and leave a "vent " hole at each end for the foam to come out 

NOw i pour the foam on one side close up the mold - I cant vaccum it because all the foam may go into vacuum

I could just clamp i guess but then how does each side of the carbon stick to each other and give me a finished surface

ralphey
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Hi,
cure both sides separately then put the moulds together and pour in the foam, I'd recomend a foaming epoxy as it will be more durable and have better material properties than some (cheaper) 2 part foams.

Chris
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
When you design your pattern and mould for each side, you can design in a flange for bonding the two parts together. Recess the flange by the thickness of the carbon plus a bit for glue.  That way you have an area of overlap you can bond to secure the two halves together.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search