I am planning to make A arms and the push-rods using carbon fibre tubes.
How should I chose the inner dia and outer dia of the tubes so as to avoid failure.
provided the forces are
1903.803297 front lower A
2166.240985 rear lower A
414.642784 front upper A
394.6610908 rear upper A
all forces in lbs