Hi everybody


Author
Message
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Great to have you here!
If you have any questions, just ask Wink

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Zorongo
Zorongo
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 40, Visits: 330
Smile  I´m new here after Reading to you for any week.




English is not my mother language so, excuse my mistakes   Whistling

Neither my pc is, so that many times the corrector decides to add accents or do any other changes. Again excuses !




I have worked for many years building composites. In a begining epoxy sándwich parts, between 8 and 12 m typically. Carbon unis, kevlar, PVC, Nomex, etc

Then a bit of industrial composites with vinyl and polyester, and now carbón + epoxy again.




We are building cosmetic carbón parts. Under vacuum. No pinholes nor voids allowed and so, may wasted time and mterials !




I´m thinking on changing our process into infusión.




I´m anxious to learn from your experience and hope I can help to any of you sharing mine.




See you later ! Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search