Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Hand Layup
»
Wrinkles when vacuum-bagging :(
Wrinkles when vacuum-bagging :(
Post Reply
Like
2
Wrinkles when vacuum-bagging :(
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
brummelisa
brummelisa
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 20,
Visits: 144
Hi,
I just made a toptube on a bike-frame. The tube was made from a plug that I vacuum-bagged.
I noticed that I have got a couple of "bumps" that I wonder how I can remove and to prevent for happening next time.
Can I just sand it off (I will add several layers on top of it)?
I wrapped the CF in two layers and was very careful that I didn't had any wrinkles. I used peel-ply and breather.
My concern is how can I assure not to have wrinkles when I'm vacuum-bagging? I mean when the vacuum is applied I don't have super-control if the CF wrinkles (since I can't see it through the breather).
Should I only wrap one layer at a time? (I intend to wrap 6-10 layers depending on which part I'm making.
Note, that I don't use a mold, but a plug and you can see the wrinkles in the attachment
/ Marcus
Attachments
bild 2.JPG
(
707 views,
1.00 MB
)
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Wrinkles when vacuum-bagging :(
brummelisa
-
13 Years Ago
Can you use shrink tape instead of vacuum?
progetto
-
12 Years Ago
Marcus - Just to clarify, is the peel-ply and breather being applied on the finish side of the...
AlpacaChris
-
12 Years Ago
Time ago I did any composite tubetrials. The problem is that before applying vcuum, you have a...
Zorongo
-
12 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search