Hi,

I just made a toptube on a bike-frame. The tube was made from a plug that I vacuum-bagged.

I noticed that I have got a couple of "bumps" that I wonder how I can remove and to prevent for happening next time.

Can I just sand it off (I will add several layers on top of it)?

I wrapped the CF in two layers and was very careful that I didn't had any wrinkles. I used peel-ply and breather.

My concern is how can I assure not to have wrinkles when I'm vacuum-bagging? I mean when the vacuum is applied I don't have super-control if the CF wrinkles (since I can't see it through the breather).

Should I only wrap one layer at a time? (I intend to wrap 6-10 layers depending on which part I'm making.

Note, that I don't use a mold, but a plug and you can see the wrinkles in the attachment

/ Marcus
Attachments
bild 2.JPG (702 views, 1.00 MB)
Reply
progetto
progetto
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 6, Visits: 231
Can you use shrink tape instead of vacuum?