Hi, one issue of trying to heat cure one section when using CF is that carbon is a very good heat conductor so if you heat one area it is likely the heat will migrate to the rest an area of the part which only has low or medium temp resin.
Also, unless you are using prepreg it would be nearly impossible to avoid mixing the resins so you need to look at resin compatibility (which there will most likely be no manufacturer data for.