Loopback Kevlar and Fleece


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The fleece will stretch a little on all directions due to the more random nature of the fabric.

The loopback will stretch diagnolly more than along the fabric length due to the more even 0 and 90 degree thread orientation.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
ld7
ld7
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 1, Visits: 7
Just wondering how stretchy these are and if they stretch in all direction or not.

Thanks!