fibreglass and epoxy the same as carbon fibre and epoxy?
fibreglass and epoxy the same as carbon fibre and epoxy?
Post Reply
Like
9
fibreglass and epoxy the same as carbon fibre and epoxy?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
wozza
wozza
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
carbonfibreworks (15/11/2013)
Warren
Empty your pm box as i can not message you
Chris
www.carbonfibreworks.co.uk
It is empty. Here is my email just in case.
carboncopiesltd@yahoo.co.uk
Carbon
Copies Ltd
Reply
Like
8
carbonfibreworks
carbonfibreworks
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Warren
Empty your pm box as i can not message you
Chris
www.carbonfibreworks.co.uk
Reply
Like
8
wozza
wozza
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 688,
Visits: 5.4K
If you are going to use CSM and Epoxy Resin remember the CSM needs to be "powder bound" not "emulsion bound". Epoxy won't break down the "emulsion" holding the fibres together.
Warren
Carbon
Copies Ltd
Reply
Like
9
baja_patient
baja_patient
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 135,
Visits: 1.6K
Stingy or not, its just not worth the effort and time (which are also worth money) to use inferior materials.
Cheers
Reply
Like
9
jontex
jontex
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Awaiting Activation
Posts: 4,
Visits: 91
thank you for the help! Im gonna make a couple of shin guards for alpine skiing. Im a little too stingy to use the carbon fibre so im going to try out the fibreglass
Reply
Like
9
wojtepanik
wojtepanik
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 102,
Visits: 582
Yeah, sure procedure is the sam but instead of using cf you lay fiber glass cloth, but there is no sense in laminating some small fg part with epoxy resin. You should use poly resin with gelcoat and some light cloth or csm.
Bye!
Wojtek from Poland
~~~Everytime I hear sound of demoulding part I have eargasm~~~
Reply
Like
9
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
you can use any weave you want. Sometimes I use fiberglass to test the surfacefinish of my proces/muold before using the expensive Carbonfiber
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
8
jontex
jontex
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 4,
Visits: 91
Hey!
Im going to make a part out of fibreglass and epoxy, is there something different or can i do it the samy way as with carbon fibre?
Im thinking of doing it this exactly this way, but with fibreglass instead of carbon fibre,
Thanks for your answers!
Tags
carbon
epoxy
fibreglass
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search