Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Laying cloth into complex moulds
Laying cloth into complex moulds
Post Reply
Like
3
Laying cloth into complex moulds
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
FLD
FLD
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 468,
Visits: 2.7K
I'm making a hard top roof for my car and the inner part is quite a complex shape with lots of complex curves and sharp returns. In this case pro-finish is not my friend as its just not mobile enough. I'd appreciate some pointers on how you guys deal with these sort of problems.
This is a pic of the plug, the white is the mould for the outer part, the blue is the plug for the inner piece that I'm moulding.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Laying cloth into complex moulds
FLD
-
12 Years Ago
Hi, Come on, it is not that complex ;) or maybe I just can't see it on the picture, I think that...
wojtepanik
-
12 Years Ago
:D Love the banter! The sharp returns are the squares in the middle have a 1/2 in 90 degree return...
FLD
-
12 Years Ago
If you are careful, use adequate spray tack n regular 2x2 twill, you should easily be able to get a...
baja_patient
-
12 Years Ago
Thanks for the pointer, exactly what I was after.
FLD
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search