Opps, sanded through gelcoat on female mould, how best to repair?


Opps, sanded through gelcoat on female mould, how best to repair?
Author
Message
Leew
Leew
Supreme Being (435 reputation)Supreme Being (435 reputation)Supreme Being (435 reputation)Supreme Being (435 reputation)Supreme Being (435 reputation)Supreme Being (435 reputation)Supreme Being (435 reputation)Supreme Being (435 reputation)Supreme Being (435 reputation)
Group: Forum Members
Posts: 33, Visits: 187
Ok, I have made a female mould using the EC epoxy tooling gelcoat and then a few layers of standard glass fabric with laminating epoxy.  I had a few imperfections in the mould so sanded them out but I've gone through the gel-coat and into the fibers in a few places.  I was wondering what is the best way to repair this?  Is it possible to add some wax to the gelcoat to make it behave like a top coat for example and use that on top of the affected areas? 
Many thanks, lee.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search