			            Hi Matthieu,
  Thank you, nice to talk to you again.
  You're quite right that side projections onto a solid foam block is an alternative method however what this technique would not do is give you the all-important round profiles of the inlet mouth for example, or any of the detail for the internal scoops (on the top or the bottom). For a more simple shape this would often be the way to go, for a shape like ours then we made a choice to go with the extra detail and reference accuracy that the profile skeleton provides and for something more complicated yet then we would certainly choose the profile skeleton method as often a lot of important detail would be lost if we only had basic projections.
  All the best, Matt                  
			            
  				
			            Matt Statham Easy Composites / Carbon Mods - Technical Sales                     
                     
                                            
                         
                    
                  
             |