Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Significant oil making it's way to the vaccum Chamber
Significant oil making it's way to the vaccum Chamber
Post Reply
Like
2
Significant oil making it's way to the vaccum Chamber
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 380
That's strange. My vacuum pump is almost twice as cheap as the one offered here but it has an anti-suck back feature so no matter what, no oil gets sucked back
Reply
Like
3
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
That is correct, turn the valve to shut, then flick off the pump.
When turning the pump on, switch on then open the valve.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
jeangui
jeangui
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2,
Visits: 7
Thanks Warren for the prompt feedbacK.
So if I understand correctly, one needs to close the valve before switching it off. Correct ?
What about when turning it on. Does it matter if the valve is open or closed ?
Thanks again.
Jean
Reply
Like
2
Warren (Staff)
Warren (Staff)
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
Do you shut the valve on the pump when you turn the pump off??
If not, oil gets sucked back through the pump and the lines into the chamber.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
2
jeangui
jeangui
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 2,
Visits: 7
Hello,
I just received
a new
Vacuum Degassing System - Small Vacuum Pump.
After toping the Oil as per instructions, I am running some trial runs. During these, I noticed a significant amount of Oil in the vaccum chamber (see image below).
Otherwise the pump pulls a vacuum.
Is there a step I am missing which is leading to this issue ?
Many thanks,
Jean P
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search