Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Surface finish for easy-lease
Surface finish for easy-lease
Post Reply
Like
3
Surface finish for easy-lease
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Leew
Leew
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 33,
Visits: 187
What kind of surface finish is required for easy lease to work effectivly?
Does the surface have to be finished to a high gloss, or would a 400 grit finish for example still work OK?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Surface finish for easy-lease
Leew
-
12 Years Ago
hi, there is a rule : better mould finish = better final part finish. When the mould is glossy it...
wojtepanik
-
12 Years Ago
I'm not that bothered about the finish of the part, it's going to be painted so does not need to be...
Leew
-
12 Years Ago
I think that 800 would be ok but just to be sure apply couple more layers of agent, or put some more...
wojtepanik
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search