Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Where could I get the pigments for silicone rubber?
Where could I get the pigments for silicone rubber?
Post Reply
Like
9
Where could I get the pigments for silicone rubber?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
boshuzhang
boshuzhang
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 3
I have searched the website but the only results given were for epoxy, Polyurethane and Polyester. Anyone has any idea for this?
Tags
pigment
Silicone Rubber
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Where could I get the pigments for silicone rubber?
boshuzhang
-
13 Years Ago
We don't at present stock any pigments for silicone rubbers. The reason being that our silicones are...
Warren (Staff)
-
13 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search