Excellent. Thanks very much. 
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As for the resin choice the ultimate resin would probably be our rapid repair resin as this has incredibly high bond and flexural strength (it also cures very quickly which is useful especially if you are working with the resin outside) Obviously this performance comes at a price and I would imagine that our EL2 resin system would do the job perfectly well if you are more price sensitive.

In terms of fillers, we do not stock wood flour but it is available from a number of wood suppliers from a quick search on google.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Funfrock
Funfrock
Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)Forum Member (44 reputation)
Group: Forum Members
Posts: 2, Visits: 4
Hi I am planing to build a small rowing boat and was wondering which epoxy resin I should use. The construction will be stitch and glue and made from plywood with fibreglass joints and outer skin. 

I also need a bulking agent ie wood flour, do you sell this , if not could tell me where I would find it 

Hope this makes sense. 

Many thanks. 