As long as you have rubbed down using 80 to 120 grit you should be fine but may be you should test first ,the only issue I could see is epoxy reacting with contaminated paint,I use epoxy on rotten wood to harden the wood the fill and paint,the problem at the moment is ici and all manufactures are struggling to find a formula to comply to eu leg,regarding paint that why ther paint is crap,when it becomes water based you might as well use emulsion.good luck. 
Graham Hurley
Graham Hurley
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 2
I've got a timber framed property where the timber is failing.
Painting has not formed a waterproof surface.
Can I apply epoxy coat to painted surface to try and create weatherproof layer ???
Thanks
Graham Hurley
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search