I wouldnt recommend carbon fibre or one of our flexible resins for that kind of application.

Drive belts and conveyor belts usually use a special compound of rubber as well as having kevlar or steel wire/belt reinforcement within them.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
hmdqasemi
hmdqasemi
Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)Junior Member (7 reputation)
Group: Forum Members
Posts: 1, Visits: 3
Dear engineer,

I want to make conveyor belt that should be have enough flexible.other specification that is important for me is temperature that should support about 130 C.
Could you please introduce material?
Could you please send me datasheet?

Thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search