Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Uni-Mould
»
does coupling coat need to set before tooling resin layup?
does coupling coat need to set before tooling resin layup?
Post Reply
Like
7
does coupling coat need to set before tooling resin layup?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
James66
James66
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 10,
Visits: 99
Hi
making a mould + havnt used uni-mould system before,
I know the gel coat has to cure before coupling coat but does the coupling coat need to cure before tooling resin + csm layup?
Cheers for the help
james
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
does coupling coat need to set before tooling resin layup?
James66
-
13 Years Ago
After about 2 to 3 hours should be enough time time depending on temperature,the coupling coat does...
Shaneer22
-
13 Years Ago
Ok cheers for that, thank you
James66
-
13 Years Ago
Just to check is the coupling coat is taken to tack or fully cured befor the reinforcement is added
ceebmoj
-
11 Years Ago
Fully cured mate.
Hanaldo
-
11 Years Ago
I always make sure its not fully cured lets say (+24h) but laminate on top of it with the tooling...
matthieutje65
-
11 Years Ago
Yeh spot on Matthieu, probably should have been more clear with my response. I meant fully hardened...
Hanaldo
-
11 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search