for me, it'a a bad idea use the storage in photo. You can ask to a storage factory a new factory without a bottom, then do the door and settle and check the welds. Rimember, an autoclave is a big bomb...if you have a 1 m diameter door, with 5 bar of internal pressure, you have many tons of thrust....
|